How to improve the curing rate of silicone products

Information Sources: | Release date: 2017-12-28 | Page views:
Key words:How to improve the curing rate of silicone products

Silicone products quality is now more and more high, in fact, some measures to the manufacturers, in order to reduce the cost of a certain, during vulcanization, this to a certain extent it can significantly improve the work efficiency, at the same time also can reduce costs, why not, but there is a problem is very difficult, that is speed.

Silica gel products vulcanization rate:
1, household appliances rubber hose manufacturer introduce can be appropriately increased silicone raw materials added in the curing agent, or choose fast curing agent, in order to speed up the vulcanization silicone products, shorten the molding time. Can improve the forming when curing temperature appropriately, but generally the structure of the product will be different, so need to test to determine the specific temperature.

2, change the silicone raw materials discharge way, try to make the mold in the process of pressurized, silicone material can go as far as possible with the mold wall. Forming the operator to speed up the operation, to minimize the time outside, in order to stabilize the silicone mold temperature, improve the cure rate of silica gel products.

Number 3, change the exhaust gas and the exhaust stroke. As a rule, the larger the exhaust stroke, the exhaust, the more conducive to exhaust. But it is not the case, we need according to the structure of the product to decide, some silicone products exhaust stroke, it will appear bubbles, etc.

Appliances rubber hose factory is introduced in addition, can use other methods can improve the efficiency of production, change the number of exhaust gas and the exhaust stroke, the debugging work experience requirements is higher, because as a rule, the larger the exhaust stroke, the exhaust, the more will be more conducive to exhaust. But it is not the case, need according to the structure of the product to decide, some silicone products exhaust stroke a bubble will appear adverse instead, and down is solved.




Related articles
Related Products
  • F-006
    F-006
  • F-005
    F-005
  • F-004
    F-004
  • F-003
    F-003
  • F-002
    F-002
  • G-001
    G-001
  • C-013
    C-013
  • E-013
    E-013
Quick Links
Home page
About us
Product center
News center
Contact us
Research center
Contact information
|Baizhang Industrial Park, Changzhou City, Jiangsu Province
|ss@czrubber.com
|0086-519-85860568
Online message
Name
Tel
E-mail
Message content
Links:
Top